Super Alloy Shackles

| All Dimensions in inches. D=Bow Diameter d=Pin Size a= inside width C=inside length r=radius |
| WLL |
D |
d |
a |
C |
Width |
| Metric Tons |
Bow Dia |
Pin Size |
In Width |
In Length |
of bow 2r |
Pkg Qty |
Pkg Wgt lb |
LACLEDE Part Number |
| 30 |
1-1/2 |
1-5/8 |
2-3/8 |
5-3/4 |
3.90 |
1 |
18 |
7723-038-80 |
| 40 |
1-3/4 |
2 |
2-7/8 |
7 |
4.96 |
1 |
31 |
7723-045-80 |
| 50 |
2 |
2-1/4 |
3-1/4 |
7-3/4 |
5.44 |
1 |
42 |
7723-050-80 |
| 80 |
2-1/2 |
2-3/4 |
4-1/8 |
10-1/2 |
7.09 |
1 |
84 |
7723-065-80 |
| 110 |
3 |
3-1/4 |
5 |
13 |
7.49 |
1 |
130 |
7723-075-80 |
|